Dryers, Size Press, Calender, and Reel
Learn how steam-heated dryer cans evaporate the last water, what the size press and calender add, and how the sheet is wound into a parent roll and slit into customer rolls.
The Dryer Section
The dryer section is the longest, most expensive part of the paper machine. A large linerboard machine may have 50 to 100+ dryer cans — cast-iron or steel cylinders, often 1.5–1.8 m in diameter, heated from inside by steam.
The sheet snakes over and under the cans, held tight against them by dryer fabrics. Heat passes from the steam, through the can shell, into the sheet, and the water evaporates into the surrounding air. A hood encloses the section and captures that moist air for heat recovery.
Getting Water and Heat Out of the Cans
Inside each can, the steam gives up heat and condenses. If the condensate isn’t removed, it forms a layer that insulates the shell and reduces drying. A siphon picks up the condensate, and a steam-and-condensate system cascades steam from higher-pressure sections to lower ones.
Dryers are grouped into sections with separate steam pressures so operators can control the drying curve — gentle at the wet end to avoid picking and sticking, hotter in the middle, and controlled at the end to hit target moisture.
Typical Targets
Paper leaves the dryers at about 5–8% moisture (92–95% solids). Too dry wastes steam and makes the sheet brittle; too wet risks mold, curl, and poor converting.
Common mistake: running a couple of points drier than target “just in case.”
Overdrying wastes steam (the most expensive water you’ll ever remove), makes containerboard brittle so it cracks on the corrugator’s scores, and sells less water — paper is sold by weight, so overdrying literally gives product away. Hit the target, and level the CD moisture profile instead of drying everything to protect the wettest streak.
The Size Press
Partway through the dryers, many machines have a size press, where a starch solution is applied to the sheet surface and then re-dried.
- Puddle size press: the sheet passes through a pond of starch between two rolls. Simple but can cause sheet breaks at high speed.
- Metering (film) size press: a thin, measured film of starch is applied to the rolls first, then transferred to the sheet. Handles high speed and gives more uniform pickup.
Surface starch increases surface strength (so ink doesn’t pick fibers off), stiffness, and for containerboard, compression strength — critical for box performance.
Calendering
A calender is a stack of hard rolls that the dry sheet passes through. Pressure smooths the surface and evens out thickness.
- Improves smoothness and printability
- Levels the caliper (thickness) profile across the width
- But reduces bulk and stiffness — so board grades are calendered lightly
Glossy coated papers often go through a supercalender or soft-nip calender offline or online for a high-gloss finish.
Reel and Winder
At the end of the machine, the sheet is wound onto a steel spool at the reel (often a Pope reel) to make a parent roll (also called a jumbo roll or machine reel). A full parent roll can be the full machine width and weigh tens of tons. When it’s full, the sheet is transferred to a new spool at full speed — a turn-up.
The parent roll goes to the winder, which unwinds it and slits it into customer rolls of the ordered widths and diameters.
- 1 Parent roll
Full machine width, wound at the reel
- 2 Unwind
Parent roll mounted on the winder unwind stand
- 3 Slit
Rotating knives cut the web to ordered widths
- 4 Rewind
Sets of rolls wound on cores to target diameter
- 5 Wrap & label
Rolls wrapped, weighed, and barcoded
- 6 Ship
Clamp trucks load trucks and railcars
Planners use deckle (trim) optimization to combine customer orders across the parent roll width while minimizing waste. The narrow edge strips left over become trim that’s repulped as broke.
Roll Quality
A customer roll must unwind smoothly on a corrugator or press. Winders control wound-in tension to avoid:
- Soft rolls that go out of round in storage
- Hard rolls that crack or burst at the core
- Telescoping layers and crepe wrinkles
Key Takeaway
Steam-heated dryer cans evaporate the last ~50% water — the most expensive water removal in the mill. The size press adds surface starch for strength, the calender smooths and levels caliper at some cost to bulk, and the reel and winder turn the sheet into customer rolls.
Look up a photo of a paper roll label online (search “paper roll label linerboard”). Identify the grade, basis weight or grammage, width, diameter, weight, and roll ID. Every one of those fields was set at the reel or winder. The roll ID lets the mill trace any customer complaint back to the exact parent roll and time it was made.
1. What heats a typical paper machine dryer can?
Steam condenses inside the cans, releasing heat through the shell into the sheet.
2. Why must condensate be removed from dryer cans?
A layer of condensate acts as an insulating blanket. Siphons remove it to keep drying efficient.
3. What does surface starch at the size press improve in containerboard?
Surface starch strengthens the surface and improves stiffness and compression — critical for boxes.
4. What is a trade-off of heavy calendering?
Calendering compresses the sheet, improving smoothness but reducing bulk and stiffness.
5. What does the winder do?
The winder unwinds the parent roll, slits it, and rewinds customer rolls.