Marine Steels, Aluminum, and Dissimilar Metals
Module 4 · Materials and Quality

Marine Steels, Aluminum, and Dissimilar Metals

Learn the classification society steel grades (A, D, E and AH36/DH36/EH36), why toughness matters at sea, preheat and hydrogen control, marine aluminum alloys and how to weld them, and how bimetallic transition joints prevent galvanic corrosion.

Ship Steel Is Not Just “Steel”

Hull steel must be strong, weldable, and tough: able to resist cracking when cold and impacted. Classification societies such as ABS (American Bureau of Shipping), DNV, and Lloyd’s Register set grades that steel mills certify.

Ordinary-Strength Grades

GradeToughnessTypical use
ABasicGeneral hull structure in less critical areas
BBetterThicker plates or moderately critical areas
DTested for impact toughness at lower temperatureMore critical areas, such as the sheer strake and bilge strake on many ships
ETested at even lower temperatureMost critical areas and cold-service ships

Higher-Strength Grades

AH32, AH36, DH36, EH36 (and others) have higher yield strength (the “32” and “36” relate to about 315 and 355 MPa minimum yield) with the same letter-based toughness levels. Higher-strength steel lets designers use thinner plate, saving weight.

Grades are stamped or stenciled on the plate with the heat number. The mill certificate traces it. Using the wrong grade in a critical area is a serious nonconformance.


Why Toughness Matters

Steel can become brittle in cold temperatures. Famous early welded ships cracked in cold seas when brittle steel met sharp corners and weld defects. Modern grades, careful detail design (no sharp notches), and sound welds prevent it.


Preheat and Hydrogen Control

Hydrogen in a weld can cause cold cracking (delayed cracking) in the heat-affected zone, especially in thick plate, higher-strength steel, and restrained joints.

Controls:

  • Low-hydrogen consumables, stored correctly (Lesson 3.1)
  • Preheat to the temperature in the welding procedure; it slows cooling and lets hydrogen diffuse out
  • Dry surfaces; remove moisture, frost, oil, and paint
  • Maintain the specified interpass temperature range

Preheat requirements depend on the steel’s carbon equivalent, its thickness, and the hydrogen level of the process. Measure with temperature-indicating crayons or contact thermometers at the specified distance from the joint.


Marine Aluminum

Aluminum is common for fast ferries, patrol boats, workboats, fishing vessels, and superstructures, because it’s light and resists seawater corrosion.

AlloyFormNotes
5083, 5086, 5456Plate and sheetMarine-grade magnesium alloys; good weldability and corrosion resistance
6061, 6082Extrusions (stiffeners, profiles)Heat-treated; lose significant strength in the heat-affected zone when welded

Common filler wires are 5356 and 5183.

Welding Aluminum

  • Clean the oxide: aluminum forms a tough oxide film that melts at a much higher temperature than the metal underneath. Use a dedicated stainless steel brush (never one used on steel) and clean solvent.
  • GMAW (often pulsed spray) with argon (or argon-helium) shielding; a push technique.
  • Use push-pull or spool guns because soft aluminum wire buckles in long conduits.
  • Watch for porosity (hydrogen from moisture or hydrocarbons) and hot cracking (wrong filler).
  • No color change warning: aluminum doesn’t glow before it melts, so it’s easy to burn through.

Dissimilar Metals and Galvanic Corrosion

When two different metals touch in seawater, they form a battery. The less noble metal corrodes faster. Aluminum next to steel, bronze, or stainless will corrode.

To join an aluminum superstructure to a steel deck, yards use bimetallic transition joints: explosion-bonded strips with steel on one side and aluminum on the other. Steel is welded to steel, and aluminum to aluminum. Keep welding heat from overheating the bond line, per the maker’s limits.

Isolate other dissimilar contacts with insulating gaskets, sleeves, and coatings.

⚠️ Common Pitfall: One Brush for Everything

Common mistake: using the same wire brush and grinder disc on steel and aluminum.

Steel particles embedded in aluminum create galvanic corrosion pits, and contaminants cause porosity. Keep separate, labeled tools for aluminum, stainless, and carbon steel.


Key Takeaway

Ship steels are graded for toughness (A, B, D, E) and strength (AH32/AH36 and up). Control hydrogen with low-hydrogen consumables, preheat, and dry surfaces. Marine 5xxx aluminum plate is very weldable; 6xxx extrusions lose HAZ strength. Clean aluminum oxide with dedicated tools. Use bimetallic transition joints to join aluminum to steel.

🧪 Try It: Read a Plate Marking

A plate is stenciled: ABS DH36 · Heat 4B7721 · 20 mm.

  1. Who certified it? (ABS.)
  2. What strength and toughness level? (Higher-strength (about 355 MPa minimum yield) with D-level toughness.)
  3. Why record the heat number? (It traces the plate to the mill certificate’s chemistry and test results.)
  4. Would you expect preheat to be considered? (Possibly. 20 mm higher-strength steel may require preheat depending on the procedure, carbon equivalent, process, and conditions.)
🧠 Knowledge Check

1. Between ABS Grade A and Grade E steel, which has better low-temperature toughness?

2. Why is preheat used on thick or higher-strength steel?

3. How is an aluminum superstructure typically joined to a steel deck?

4. Why use a dedicated stainless brush for aluminum?